Abstract
Atomic layer deposition (ALD) is a surface synthesis technique that is characterized by self-limiting reactions between gas-phase precursors and a solid substrate. Although ALD processes have been demonstrated that span the periodic table, a greater understanding of the surface chemistry that affords ALD is necessary to enable greater precision, including area- and site-selective growth. We offer new insight into the thermodynamics and kinetics of the trimethylaluminum (TMA) and H2O ALD half-reactions with calibrated and time-resolved in situ pyroelectric calorimetry. The half-reactions produce 3.46 and 2.76 eV/Al heat, respectively, which is greater than the heat predicted by computational models based on crystalline Al2O3 substrates and closely aligned with the heat predicted by standard heats of formation. The pyroelectric thin-film calorimeter offers submillisecond temporal resolution that uniquely and clearly resolves precursor delivery and reaction kinetics. Both half-reactions are observed to exhibit multiple kinetic rates, with average TMA half-reaction rates at least 2 orders of magnitude faster than the H2O half-reaction kinetics. Comparing the experimental heat with published computational literature and additional first-principles modeling highlights the need to refine our models and mechanistic understanding of even the most ubiquitous ALD reactions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.