Abstract

AbstractThe resistance of the anodic PbO film formed on lead at 0.9 V (vs. Hg/Hg2SO4) in 4.5 mol/dm3 H2SO4 was measured using alternating‐current impedance method. The resistance of the anodic PbO film was found to be close to that of the interstitial liquid among the PbO particles in the film, suggesting mat the interstitial liquid may serve as the major passage for ion transportation during the film growth.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.