In this paper, through the influence of baking temperature and time on the hydrogen release of silicon carbide particle reinforced aluminum matrix composite (SiCp/Al) base plate, titanium alloy enclosure and its package shell, the hydrogen control process of package shell is proposed. The results show that increasing the dehydrogenation temperature and prolonging the dehydrogenation time can reduce the hydrogen release from the package shell. By using this hydrogen control process, the internal hydrogen release of the package shell under the baking condition of 250℃ and 48 hours cannot be greater than 2000ppm, which can effectively improve the consistency of the hydrogen release of the product, and the impact on the appearance quality, adhesion and weldability of the coating is acceptable, meeting the product use requirements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.