Abstract
In the present research an attempt has been made to replace some part of fine aggregate (sand) by an industrial waste, the industrial waste under investigation is produced when the PVC pipes are cut into the desired sizes, it is a very thin flaky substance having a specific gravity of 1.5.This material is very voluminous in nature, so it reduces the workability of concrete if used in large percentage. So this material cannot be used in very large quantities but it can successfully replace sand up to 20 percent when used in pavement blocks. Experimentation was done at a water-cement ratio ranging from 0.43-0.35.Compressive strength of the concrete has been evaluated at 7 days, 14 days 21 days and 28 days. Results of the investigation indicate that compressive strength of the concrete decreases as the percentage of PVC waste material increases.7 day strength of the concrete has varied from 35.55 MPa to 70.01 MPa and 28 day strength has varied from 56.7 MPa to 76 MPa. Water absorption was well within the limits and varied from 4.67% to 7.26% by mass. The results revealed that this waste material can satisfactorily replace sand in small amount also it is a great way to dispose of the waste and hence is a step forward in the quest for a greener concrete.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Emerging Research in Management and Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.