Re-oxidation of thermally nitrided SiO2 thin films was studied. The SiO2 growth rate at re-oxidation is reduced until a certain time (the “oxidation delay time” or “ODT”) has passed. During the ODT, thermally nitrided SiO2 at the Si-SiO2 interface is re-oxidized. the ODT is the time required for complete oxidation of nitrided SiO2. Re-oxidation of thermally nitrided SiO2 thin films is limited not by diffusion of oxidizing species, but by oxidation of nitrided SiO2. The ODT is proportional to the nitrided SiO2 thickness. Nitrided SiO2 formation at the Si-SiO2 interface is mass-transfer controlled by nitriding species through nitrided SiO2 to Si substrate. As an application of thermal nitridation of SiO2, thermal nitridation of the local oxidation of silicon (LOCOS) pad oxide can shorten the bird's beak of LOCOS.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.