Abstract

The reliability and degradation mechanisms of 70 nm gate length metamorphic InAlAs/InGaAs HEMTs for low noise applications will be presented and discussed. Based on a 10% g m max failure criterion, a median time to failure of 10 6 h and an activation energy of 1.3 eV in air were found. By comparing the electrical device characteristics before and after stress, gate sinking, ohmic contact degradation, and hot electron degradation were found to be the major failure mechanisms. The stress induced platinum diffusion into the semiconductor was quantified by cross-section TEM.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.