Abstract

The release of mercury vapor was determined from eleven different amalgams exposed to externally induced corrosion by galvanic contact with a dental casting gold alloy. The electrolyte was an artificial saliva solution at 37°C. The corrosion rates of the amalgams could be divided into two groups corresponding to the grouping into conventional and high-copper materials. The mercury release rate decreased during the 24 h test period for all the amalgams except one containing indium. There was no significant difference in the total mercury release between the conventional and high-copper amalgams as groups. The same applied for the individual products, except the one containing indium, which released significantly more mercury vapor than the two products with the lowest release.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.