Abstract
A Ru–SiO2 intermediate layer was introduced between the Ru and recording layers to reduce the intermediate layer thickness of CoCrPt–SiO2 perpendicular recording media. A structural analysis revealed that the Ru–SiO2 intermediate layer enhanced the oxide segregation in the initial growth region of the recording layer. A micromagnetic simulation and magnetic property measurements indicated that the Ru–SiO2 intermediate layer reduced the intergranular exchange coupling in the initial growth region of the recording layer without magnetic anisotropy degradation. We reduced the intermediate layer thickness down to 9.1nm by using the Ru–SiO2 intermediate layer while maintaining the signal-to-noise ratio.