A new composition of bioactive glass, in the quaternary system SiO2–CaO–Na2O–P2O5, was synthesized using melting and sol–gel routes. The prepared glass, 52S4: (wt.%) 52% SiO2–30% CaO–14% Na2O–4% P2O5, was soaked in Simulated Body Fluid (SBF) in order to evaluate the kinetic reactivity of this glass versus the synthesis mode. The obtained results have shown that 52S4 is a bioactive glass if it is prepared either by melting or sol–gel methods. The bone-like apatite was formed at the glass surface prepared by sol–gel route after 2h. However, the formation of this apatite was delayed to 1day when the glass was prepared by melting method. In addition, this apatite was crystallized, after 30days soaking in SBF, only if the glass is prepared by melting route. The glass prepared by sol–gel method was more resorbable and leads to silica gel formation up on amorphous apatite layers at any time. So, this silica gel inhibited the crystallization of amorphous apatite.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.