What is the rate of consumption of Cu in soldering reactions has been a critical question in electronic packaging technology. The Cu films are consumed by Cu–Sn compound formation. Because the Cu thickness is limited and the rework of a solder joint requires a layer of unreacted Cu, the loss of Cu in soldering must be under control. At the solder interface, Cu–Sn intermetallic compounds do not form layered structures. Rather, the Cu6Sn5 phase grows as scalloplike grains into the molten solder and ripening occurs between the grains. Therefore, it has been difficult to determine the compound growth rate, and in turn the Cu consumption rate. Using cross-sectional and top-polished samples, we have measured the total volume of Cu–Sn intermetallic compounds formed between eutectic SnPb alloy and Cu substrate as a function of reflow time and temperature. We have deduced that after 1 min reflow, for example, the thickness of Cu consumed was about 0.36, 0.47, and 0.69 μm at 200, 220, and 240 °C, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.