Radiation hardness of a 4×4×24 cm 3 PbF 2 crystal has been studied for doses up to 10 5 Gy. Radiation resistivity was examined by the measurement of optical transmission through the lead fluoride crystal before and after gamma-ray irradiations. The results have been compared with radiation hardness measurements for a 4×4×40 cm 3 Pb-glasses SF 5 and SF 6 and a 3×3×6 cm 3 CeF 3 scintillation crystal, as well. Complete recovery of radiation damage was observed a few day after the irradiations.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.