Abstract
The SWNTs with a carbon content of approximately 3% were synthesized via the disproportionation of CO over a CoMo/SiO2 catalyst. The three sequential steps, including acid treatment, silica dissolution, and froth flotation, were proposed for the purification of the as-synthesized SWNTs. The pretreatment step for the catalyst removal by acid leaching was optimized at an HCl concentration of 6 M, 50°C, and a sonication time of 3 h, corresponding to the Co and Mo removals of 84% and 44%, respectively. For the silica dissolution, the SWNTs sample after the acid leaching step was treated with a 5 M NaOH solution at 50°C and a sonication time of 3 h, leading to a silica removal of 54%. The froth flotation was employed to separate the SWNTs from the remaining silica using SDBS as an anionic frother. The process performance was maximized at an SDBS concentration of 0.1 × CMC, an air flow rate of 120 cm3/min, and a solution pH of 5, yielding a carbon content of the purified SWNTs of 71%. It was also found that the proposed technique successfully purified the as-synthesized SWNTs sample without damaging its nanostructure.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.