The purification of lignocellulose hydrolysate is crucial for the efficient conversion of lignocellulose. In this study, weak polar poly(styrene-divinyl benzene-methyl acrylate) (PSDM) and composite absorbent org-attapulgite/poly(styrene-divinyl benzene-methyl acrylate) (PSDM-T) were prepared in situ by suspension polymerization for the detoxification of mixed hydrolysate. The org-attapulgite (O-A-T) used was functionalized with the silane coupling agent KH-570. The effect of O-A-T mass on PSDM-T was investigated. The results showed that the addition of a moderate mass of O-A-T improved the pores of PSDM-T and adsorption abilities. Furfural and 5-HMF (FS), total weak acids (WA), and soluble lignin (SL) were removed simultaneously. The adsorption capacities of PSDM-T for FS, WA and SL were 37.5 mg/g, 34.3 mg/g, and 87.7 mg/g, respectively. Correspondingly, their removal extents (R) were 72.6%, 18.1%, and 52.3%. The adsorption abilities of the PSDM-T for mixed hydrolysate was better than AB-8 (a commonly-used adsorption resin). The total decolorization rates (D) greater than 63%. The absorption property retains high adsorption activity after two cycles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.