Abstract
A heated tungsten (W) mesh, set between a pentacene source and a substrate in a vacuum chamber, was used to prepare a bulk-phase pentacene film and a pentacene-based organic semiconductor film. Since the pentacene molecules come into contact with the heated W mesh before reaching the substrate, their thermal energy is increased prior to deposition. As the mesh temperature was increased from 23 to 1200°C, the intensity ratio of bulk to thin-film phases increased from 0 to 9.7. Above 1300°C there is a notable decomposition reaction, the products of which were identified as dihydropentacene, p-distrylbenzene, and 2,2′-dimethyl-1,1′-binaphthalene. These decomposed precursors are expected to provide a potential source of large graphene sheets and graphene nanoribbons.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.