Ni (8 wt.% NiO) and NiRu (8 wt.% NiO and 1.1 wt.% RuO2) dewaxing catalysts containing a ZSM-5 zeolite were examined in the hydroconversion of 1-methylnaphthalene. The effect of the Ni incorporation method and thermal treatment of the Ni catalyst was examined. The catalysts were characterized by XRF, N2-sorption, TPR, H2-chemisorption, XPS, XRD and TPD-NH3. It has been found that the use of calcination in air for the decomposition of nickel nitrate deteriorates the activity of the Ni catalyst to the greatest extent. Ru not only enhances catalyst activity but also reduces the differences in activity resulting from the various methods of Ni catalyst preparation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.