Abstract

Ni-based catalysts show high activity for steam or CO2 reforming of methane, partial oxidation of methane, and CO or CO2 methanation. However, a challenge that Ni catalysts are facing is the high thermodynamic potential for carbon deposition, derived from CO disproportionation or CH4 decomposition. Coke deposition causes reactor blockage, and the formed carbon filaments lead to the deformation of the catalyst. Encapsulating carbon quickly induces the deactivation of Ni catalysts. In this perspective, the preparation methods for the Ni catalysts were studied by dielectric barrier discharge (DBD) plasma and thermal decomposition. The DBD plasma decomposition method and the mechanism for the preparation of the catalysts were introduced. Different Ni structures were produced by different preparation methods. The geometric structure over the Ni catalysts played an important role on carbon deposition rate and carbon morphology. DBD plasma decomposed Ni catalysts possessed improved coke resistance. The reactivity of the carbon was studied toward temperature programmed surface reaction. This perspective provides the understanding of Ni-based catalysts with coke resistance and gives the relationship of Ni structure and carbon formation.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call