Sodium-ion batteries (SIBs) are becoming an alternative option for large-scale energy storage systems owing to their low cost and abundance. The lattice oxygen redox (LOR), which has the potential to increase the reversible capacity of materials, has promoted the development of high-energy cathode materials in SIBs. However, the utilization of oxygen anion redox reactions usually results in harmful lattice oxygen release, which hastens structural deformation and declines electrochemical performance, severely hindering their practical application. Herein, a ribbon-ordered superstructured P3-type Na0.6Li0.2Mn0.8O2 (NLMO) cathode with a uniform Al2O3 coating through atomic layer deposition (ALD) was synthesized. The cycling stability and rate capability of the materials were improved by a proper thickness of the Al2O3 layer. Differential electrochemical mass spectrometry (DEMS) results clearly suggest that the Al2O3 coating can inhibit the CO2 release caused by the highly active surface of the NLMO material. Moreover, the results of transmission electron microscopy (TEM) and etching X-ray photoelectron spectroscopy (XPS) show that the Al2O3 coating can effectively prevent electrolyte and electrode side reactions and the dissolution of Mn. This surface engineering strategy sheds light on the way to prolong the cycling stability of anionic redox cathode materials.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.