Abstract
The quenching of semicoke by saturated steam (heating-gas temperature 550°C) is described. The working-moisture content Wr in the semicoke is 3.0–6.7% for the new quenching method. As a reducing agent, semicoke has good characteristics: relatively low ash content (Ad = 7.1%), low sulfur content (Sd = 0.13%) and phosphorus content (Pd = 0.029%), and high reactivity (\({K_{C{O_2}}}\) = 4.0 cm3/g s) and electrical resistivity (ρ > 1.9 × 106 Ω cm). In tests, dry-quenched semicoke performs well in the production of high-carbon ferrochrome: decreased power consumption; increased furnace productivity; decreased consumption of chromium ore; and decreased sulfur content in the ferrochrome when Karaganda coal is completely reduced by the semicoke. The optimal semicoke content in the batch is up to 50 kg.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.