Abstract

We consider the possibilities of surface hardening of zirconium and titanium alloys with conversion oxide-ceramic coatings. These coatings have been produced by the method of plasma-electrolytic treatment in alkaline solutions. We have established that the plasma temperature in discharge spark channels reaches (6–9) · 103 K. The thickness of the coatings is 100 to 120 and 30 to 40 µm, and their microhardness is ∼ 800 and ∼ 1000 MPa for zirconium and titanium alloys, respectively. The functional properties of the coatings depend on the synthesis conditions, including the electrolyte composition, the cathode and anode current densities, and also the treatment time. We have evaluated the thickness, microhardness, and wear resistance of the coatings under conditions of dry friction and cavitation as well as their fatigue strength and corrosion resistance. We have established that this treatment provides a high wear and corrosion resistance of the alloys under study with insignificant decrease in their fatigue strength.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.