Abstract

Wood cellulose nanofibrils (CNF) have been suggested as a potential wound healing material, but its utilization is limited by FDA requirements regarding endotoxin levels. In this study a method using sodium hydroxide followed by TEMPO mediated oxidation was developed to produce ultrapure cellulose nanofibrils, with an endotoxin level of 45 endotoxin units/g (EU/g) cellulose. Scanning transmission electron microscopy (S(T)EM) revealed a highly nanofibrillated structure (lateral width of 3.7±1.3nm).Assessment of cytotoxicity and metabolic activity on Normal Human Dermal Fibroblasts and Human Epidermal Keratinocytes was done. CNF-dispersion of 50μg/ml did not affect the cells. CNF-aerogels induced a reduction of metabolic activity by the fibroblasts and keratinocytes, but no significant cell death. Cytokine profiling revealed no induction of the 27 cytokines tested upon exposure to CNF. The moisture-holding capacity of aerogels was relatively high (∼7500%), compared to a commercially available wound dressing (∼2500%), indicating that the CNF material is promising as dressing material for management of wounds with a moderate to high amount of exudate.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call