Abstract
In the present investigation an attempt has been made to beneficiate goethitic iron ore containing 59.02 % Iron, 6.51 % Alumina, 4.79 % Silica, 0.089 % Phosphorus with 7.11 % loss on ignition. For this purpose, different beneficiation techniques such as gravity and magnetic separation processes have been employed. During the process two conceptual flow sheets were also developed for the beneficiation of goethite iron ore fines. In the prsent work it was possible to enhance grade of iron to 63.35, 63.18, and 65.35 % from Jigging, Multi Gravity Separation (MGS) and Wet High Intensity Magnetic Separator (WHIMS) respectively.