Abstract

Water swellable rubber was prepared by blending styrene butadiene rubber as a matrix, cross-linked poly sodium polyacrylate (PAANa) as a high absorbent water resin, copolymer styrene maleic anhydride as a compatibiliser and polyethylene glycol as an absorbent accelerant. The preparation process was described. The effects of various preparation conditions, such as amount of sulphur, ratio of silicon dioxide to nanocalcium carbonate, amount of PAANa and amount of compatibiliser, on its water absorbency and mechanical properties were investigated by orthogonal tests. The optimal reaction conditions were 2 portion (phr) sulphur, 28∶12 silicon dioxide/nanocalcium carbonate, 60 phr PAANa and 5 phr compatibiliser. Furthermore, the vulcanisation property of the rubber was measured.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.