Abstract

AbstractA water‐swellable rubber (WSR), compatibilized by the amphiphilic block copolymer, has been prepared by blending a natural rubber (NR) matrix with crosslinked sodium polyacrylate (CSP), poly(ethylene oxide)‐b‐poly(butyl acrylate) (PEO‐b‐PBA), poly(ethylene glycol) (PEG), reinforced filler, and vulcanizing agents. The preparation process was described. The microphase structure of WSR was characterized by a scanning electron microscopy (SEM) photograph. The dependence of the degree of the water‐absorbing and the water‐swelling, the water‐absorbing and water‐swelling rates on CSP, PEG, and PEO‐b‐PBA contents were investigated. The compatibilizing mechanism of PEO‐b‐PBA on WSR was studied. And the optimum composition range was identified: CSP (30–60 phr), PEG (10–20 phr) PEO‐b‐PBA (PEO/PBA = 0.36, 5 phr). © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 3120–3125, 2002

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.