Titania (TiO2) Films Having Dense and Solid Microstructure Were Prepared by Laser Chemical Vapor Deposition Using CO2 Laser. The Effects of Deposition Temperature (Tdep) and Total Chamber Pressure (Ptot) on Phase and Microstructure of TiO2 Films Were Investigated. At Ptot = 600 Pa and Tdep = 790 K, Rutile TiO2 Film Had a Polygonal Platelet Grains 2 μm in Size. At Ptot = 600 Pa and Tdep = 1010 K, Rutile TiO2 Film Had (110) Orientation and Consisted of a Truncated Polyhedron 5–6 μm in Size. At Ptot = 200 Pa and Tdep = 955 K, Rutile TiO2 Film Has a Solid Columnar Having Faceted Surface. A Dense and Solid TiO2 Film Was Obtained at Ptot = 200 Pa and Tdep = 1120 K. The Deposition Rate of TiO2 Solid Film Was Reached 240 μm h−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.