Abstract

BaCe0.7Zr0.1Y0.16Zn0.04O3-δ (BCZYZ) ceramic slurry has been prepared with different solid loading and the maximum solid loading of the slurry has been predicted as 25 vol.% using the Krieger-Dougherty equation. The slurry with the maximum solid loading has been formulated and applied as an electrolyte on porous NiO/BCZYZ tubular supports by the dip-coating method. Cells sintered at 1500°C for 10h have been characterised by Scanning Electron Microscopy (SEM) analysis. The 30μ thick, very dense electrolyte layer has successfully been achieved with some closed pores.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.