Abstract

Fine nickel(Ni) powders with controllable particle sizes were synthesized via the reduction of nickel hydrazine complex precursors of pure [Ni(N 2H 4) 2]Cl 2 and a mixture of [Ni(N 2H 4) 2]Cl 2 and [Ni(N 2H 4) 3]Cl 2 in aqueous solution. The mechanism of the formation of metallic Ni powders experiences the reduction of nickel hydroxide by hydrazine released from the ligand exchange reaction between nickel hydrazine complex and NaOH. In comparison with the method of preparing Ni powders from nickel salts, the method of making Ni powders via the reduction of nickel hydrazine complex precursors shows the advantages of using half dosage of hydrazine for complete reduction of nickel ions in solution, and the obtained Ni particles show less agglomeration and better dispersibility. Moreover, the average particle size of nickel powders can be controlled from 180 to 260 nm by adjusting the reaction molar ratio and concentration.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call