C/SiC composites were prepared by pulse chemical liquid–vapor deposition (pulse CLVD) process in 3h with liquid polycarbosilane as precursor. The microstructure and properties of the C/SiC composites were studied. The results show that the apparent density and open porosity of the C/SiC composites are 1.81 g⋅cm−3 and 8.0%, respectively. The matrix consists of β-SiC, α-SiC and pyrolytic carbon, with the grain size of β-SiC of ~42nm. And the carbon fiber adheres to the matrix with a strong interface, therefore the C/SiC composites exhibit a brittle fracture behavior with flexural strength of 138.0MPa, flexural modulus of 31.0GPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.