Abstract
Needle-shaped and film- or plate-shaped black phosphorus single crystals were prepared by an improved bismuth-flux method. The conversion of red phosphorus to white phosphorus and the growth of black phosphorus single crystals from the solution of white phosphorus in liquid bismuth were performed in an evacuated quartz-glass apparatus without breaking the vacuum. Needle crystals measured about 5 mm in length and 10 to 100 µm in thickness. The thickness of film or plate crystals ranged from 1 to 10 µm and the width was usually above 100 µm, generally increasing with decreasing thickness. Some crystal morphologies were observed and analyzed crystallographically.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.