Abstract
Tritium would be produced in the Thorium-based Molten Salt Reactor and then quickly penetrate through the structural material of GH3535 superalloy into environment at elevated temperatures. To suppress the permeation of tritium, the α-Al2O3/NiAl multilayer coatings were prepared on GH3535 by pack aluminizing (PCA) and subsequent low vacuum oxidation as tritium permeation barriers. Herein, the effects of PCA process parameters on the composition and structure of the Ni–Al coatings were characterized, simultaneously, the influence of oxidation temperature on the composition and structure of Al2O3 films were analyzed in detail. Experimental results demonstrated that the main phase of the Ni–Al layers is Ni2Al3 (or NiAl) doped with Al86Cr14. Significant amounts of Mo-aluminides were found on the surface of the samples aluminized at 1050 °C. The Ni–Al layers growth kinetic equation under 650–850 °C was empirically obtained as h = 7.07•104W1/2t1/2exp[-7.53•104/RT]. After low vacuum heat-treatment, the α-alumina films with a thickness of approximately 1 μm were formed at 1050 °C for 2 h, densely and non-porously. Meanwhile, the brittle Ni2Al3 in the transition layer was transformed into the tough NiAl, providing a self-healing capability as well as alleviating the thermal mismatch between the coating and the substrate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.