Abstract

We describe an improved sol–gel process to prepare a water-soluble oligo-( p-phenylene vinylene) (ws-OPV) doped silica composite glass. The addition of Li 2CO 3 to neutralize the composite sol and solvent extraction with cyclohexane reduces the processing time from several weeks for traditional sol–gel process to several days. The crack-free ws-OPV doped silica composite glass with the low volume shrinkage can be obtained by this process. The choice of ws-OPV ensures the possibility of this modified process. The results of fluorescence spectra indicate that the adjustable and improved emission of composite glass can be achieved, and the photostability is much better, all of which make such composite glasses of more practical significance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.