To increase the mechanical properties of PLA used for fracture inner fixation, β-calcium metaphosphate whiskers were prepared by controlled crystallization in the glass. The factors influencing the morphology of the samples, such as component, time and temperature of crystallization were discussed. Results showed that the high quality of β-calcium metaphosphate whiskers can be obtained by crystallization treating for 36 hours and washing for 48 hours at 80°C distilled water. β-calcium metaphosphate whiskers having high aspect ratios of 20-100 with diameters of 1-5μm were achieved at the optimized conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.