Abstract
Abstract MCM-48 mesoporous materials were hydrothermally synthesized according to the 22 factorial design by varying the crystallization time and temperature of the synthesis gel, and characterized by means of X-ray diffraction analysis and adsorption of N2. In the crystallization temperature and time conditions used, specific areas between 924 to 1102 m2.g-1, pore volumes between 0.015 to 0.087 cm3.g-1 and pore diameters between 3.2 to 4.0 nm were obtained. It was observed that for the syntheses performed at high temperature, the crystallization time should be reduced so that the material structure is formed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.