In this work, we use the treated PF-ADF(2 ∼ 3 mm) as the reinforcing body(fiber) and the biodegradable PBS as the matrix. The different treated PF-ADF were mixed with PBS particles according to the mass percentage of 20:80, and C-PBS, C-DF/PBS, C-ADF/PBS and C-KDF/PBS were prepared by molding process. The influence of surface treatment on the microstructure and physical properties of the fiber were discussed and the mechanical properties of the composites were compared. Also the biodegradability of the different composite was analyzed. The results showed that most of the non-cellulosic materials such as pectin were removed from C-DF, but a certain amount of pectin remains on the surface. The surface of C-ADF appeared ‘S’ groove, and the groove on C-KDF was good continuity and deep. Compared with C-DF, the tensile strength of C-ADF and C-KDF increased by 5.08% and decreased by 3.58% respectively. Compared with C-PBS, the tensile strength and bending strength of C-KDF/PBS increased by 48.32% and 25.97% respectively, and the tensile modulus and bending modulus increased by 146.45% and 128.3% respectively. The changes of biodegradability of C-DF/PBS, C-ADF/PBS and C-KDF/PBS composites were consistent, but the change of weightlessness rate of C-KDF/PBS was the smallest. The more degraded and uneven the surface of the composite, the more obvious the decrease in contact angle.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.