Abstract

Abstract In this study, a organosilicon modified waterborne polyurethane (WPU) is synthesized with polyethylene glycol 1,4-butanediol adipate ester diol (PBA) to form the soft segment, dimethylolpropionic acid (DMPA) as the hydrophilic chain extender, and isophorone diisocyanate as the hard segment to synthesize the WPU prepolymer, and aminoethyl aminopropyl dimethicone (AEAPS) as the graft chain extender. The properties of the formed WPU films are then characterized by using Fourier transform infrared spectrometry, thermogravimetric analysis, X-ray diffraction, and dynamic mechanical analysis. It is found that when the amount of AEAPS in the WPU is increased from 0 to 30 wt%, the particle size of the AEAPS modified WPU emulsion is increased from 84.8 nm to 271.9 nm and maintained high centrifugal stability. Moreover, the water absorption of the WPU film is reduced from 43.4% to 24.1%, and the hardness is enhanced from 3H to 5H, while the glass-transition temperature (Tg) of the soft segment of the modified WPU shifts from -37.4 °C to -44.3 °C, and the Tg of the hard segment shifts from 73.6 °C to 118.1 °C. Therefore, the overall performance of AEAPS modified WPU is improved.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.