Abstract
In this paper, we present a newly developed rare earth modified amorphous barium strontium titanate (Ba x Sr 1− x TiO 3) gel/silicone oil electrorheological (ER) fluid. The ER behaviors of suspensions of pure and rare earth modified amorphous Ba x Sr 1− x TiO 3 particles in silicone oil have been investigated under a dc electric field. The shear yield stress of the rare earth modified amorphous BaTiO 3 gel/silicone oil ER fluid could reach 14.9 kPa at E = 3.5 kV / mm while the leaking current density was very low, about 7.64 μA/cm 2. The ER fluids with a higher volume fraction had a higher current density and a higher shear yield stress under the same electric field. The ER fluid has a long-term stability against sedimentation. The problem of caking was not serious and the agglomerated particles could be easily broken up by strongly stirring.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.