Abstract

Nanometer scale cubic ZnTiO 3 has been synthesized by sol–gel method at a lower temperature (600 °C). X-ray diffraction (XRD) analysis shows that the average crystalline size of the sample is ∼8–10 nm. The cubic to hexagonal phase transition of ZnTiO 3 is clearly observed from the XRD patterns of the sample. The thermal behavior of the sample was characterized by the thermogravimetric/differenthermal analysis (TG/DTA), XRD patterns, and the infrared spectra (IR). Transmission electron microscope (TEM) observations of the sample reveal a high microstructural uniformity.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.