Abstract

Poly (lactic acid) (PLA)/polyethylene oxide (PEO) bicomponent fibers with porous and smooth surface on different side of the same fibers were fabricated by co-electrospinning technique. Specific solvent systems were used deliberately to induce pore formation on PLA phase. The results showed that the porous-smooth surface fibers were obtained using PLA-PEO flow rate ratio of 0.75:0.25 to 0.25:0.75 ml/hr. While, Fiber size decreased with decrease in PEO concentration and PEO flow rate ratio, the applied voltage had small effect on fiber size change. After PEO phase removal via selective dissolution with water, the C-shape PLA fibers with porous surface was generated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.