Abstract
This article focuses on the influences of austenitizing temperature and holding time on the grain sizes of 1800 MPa ultrahigh strength steel (UHS‐1800). When the austenitizing temperature increases from 900 to 990 °C and the holding time is 5 min, the austenite grain size increases from 12.60 to 20.88 μm. When the austenitizing temperature is 930 °C and the holding time increases from 3 to 9 min, the grain size increases from 13.52 to 17.22 μm. When the austenitizing temperature increases from 900 to 990 °C and the holding time is 5 min, the radiuses of the second‐phase particles increase from 15.23 to 25.36 nm. When the austenitizing temperature is 930 °C and the holding time increases from 3 to 9 min, the radius of the second‐phase particle increases from 15.72 to 20.50 nm. On this basis, a prediction model for austenite grain growth suitable for UHS‐1800 hot stamping process is proposed. The growth model of the austenite grain can accurately predict the grain growth behavior during the hot stamping process, with a maximum error of 5.35% compared to experiments.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.