Abstract

Positron beam-based Doppler broadening results on He ion-implanted FeCrCoNi show distinct changes in defect-sensitive S-parameter corresponding to the formation of helium-vacancy complexes, nucleation/ growth of helium bubbles, and finally the helium bubble rupture, with isochronal annealing. Data analyses of the positron beam-based ratio curves provide clear information on the kinetics of bubble growth and rupture. The difference data in S-parameter (ΔS), which corresponds to the bubble growth, displays a maximum at 1123 K, with annealing temperature. Comparing the ΔS value to that reported for nickel, it is concluded that FeCrCoNi has higher bubble growth resistance than nickel.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.