Abstract

AbstractFibers of the biopolymer poly(lactic acid) (PLA) and the p‐type semiconducting polymer poly(3‐hexylthiophene) (P3HT) were fabricated using the electrospinning technique at low PLA concentration (5 wt%) in CHCl3. The fibers were several millimeters long and had diameters in the range 100 nm–4 µm. Nanofibers containing 63%/37% of PLA/P3HT were electroactive, and therefore were used to construct p–n diodes whose ideality parameter was 2.4 and rectification (on/off) ratio was 400 at ±1 V. These diodes were also able to sense UV radiation and remain operable with an increase in the on/off ratio and a lowering of the turn‐on voltage. By fabricating reusable and low‐cost multifunctional diodes from PLA/P3HT, the applications of PLA as a biocompatible and biodegradable polyester are expanded to include electronic device fabrication with low environmental impact. © 2016 Society of Chemical Industry

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.