Abstract
The etch rate and surface roughness of polished and lapped AT-cut quartz subjected to hot (90, 110, and 130 degrees C), concentrated (50, 65, 80 wt %) ammonium bi-fluoride have been investigated. Having used principal component analysis to verify experimental solidity and analyze data, we claim with confidence that this parameter space does not, as elsewhere stated, allow for a polishing effect or even a preserving setting. Etch rates were found to correlate well, and possibly logarithmically, with temperature except for the hottest etching applied to lapped material. Roughness as a function of temperature and concentration behaved well for the lapped material, but lacked systematic variation in the case of the polished material. At the lowest temperature, concentration had no effect on etch rate or roughness. Future efforts are targeted at temperatures and concentrations closer to the solubility limit.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IEEE Transactions on Ultrasonics, Ferroelectrics, and Frequency Control
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.