Modeling of the constitutive behavior was undertaken for Fe- Cr-C tempered martensitic alloys. Tensile tests were carried out at room temperature and constant nominal strain rate. In order to obtain a fully martensitic structure with different prior austenite grain size, two heat-treatments, consisting of an austenization followed by a tempering, were applied to the alloys. Two tempered martensitic structures were so produced with two different prior austenite grain sizes. The as-heat-treated microstructures were well characterized by electron transmission microscopy and metallographic observations. The effect of the prior austenite grain size on the yield stress and on the strain-hardening was investigated. It was found that a moderate increase of the yield stress exists, which is certainly not consistent with a Hall-Petch relationship between the yield stress and the prior austenite grain size. The post-yield behavior was found completely unaffected by the prior austenite grain size. The stress dependence of the strain-hardening was shown to be consistent with a simplified phenomenological description of the strain-hardening based on one structural parameter, the total dislocation density. An effective mean displacement distance of the dislocations was estimated form the strain-hardening law, equal to about 10 mum independently of the prior austenite grain site. (C) 2004 Elsevier B.V. All rights reserved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.