Amorphous gallium oxide (Ga2O3) thin films were investigated as gate dielectrics for electronic device applications using plasma-enhanced atomic layer deposition. The structural and morphological properties as well as the electrical and dielectric behaviors of Ga2O3 thin films were explored. The surface morphology of the amorphous Ga2O3 thin film was highly smooth with root mean square of 0.55 nm and low defect density, which were visible to atomic force microscopy. The grazing incidence X-ray diffraction pattern showed no discernible peak, indicating that the film was amorphous. The X-ray photoelectron spectroscopy depth-profiling analysis showed that the Ga/O ratio was 0.76, slightly more than the optimum 2/3 ratio (0.67). The temperature-dependent current–voltage characteristics of the Au/Ni/Ga2O3/p-Si structure revealed that ideality factor and barrier height values decreased and increased with increasing temperature, respectively, demonstrating their high temperature dependency. Regardless of the applied frequency, Ga2O3 thin films exhibited a good dielectric constant of about ∼9 at zero bias voltage. The comprehensive capacitance–voltage analysis showed low trap densities of about 1012 eV−1 cm−2 at the Ga2O3–p-Si interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.