Abstract
In order to test some of the methods of archaeological bronze conservation, a procedure was perfected that reproduces the structure and composition of original patinas. Then the most common methods of treatment were applied on test samples thus prepared and on archaeological items. This experiment has allowed us to choose the best treatment in accordance with the following requirements: restraint of corrosion, speed of operation, lack of colour alteration and avoidance of break-up or solution of patina.