Abstract
This is the first report ever on (Mn2+–Zr4+) doped M-type lanthanum strontium hexaferrite with general formula, Sr0.85La0.15(MnZr)xFe12−2xO19 where x=0.0, 0.25, 0.50, 0.75, and 1.0, prepared by citrate auto-combustion method. These ferrites were characterized by X-ray diffraction (XRD), Scanning electron microscope (SEM), Energy dispersive X-ray spectroscopy (EDX) and Vibrating sample magnetometer (VSM). X-ray diffraction patterns show the formation of high purity hexaferrite phase without other secondary phases for all the synthesized samples. It was observed from magnetic hysteresis data that the coercive force is reduced from 5692.5Oe to 1669.2Oe with increase in doping contents but the net magnetization of the samples varies slightly from 60.6 to 55.2emu/gm. High saturation magnetization (Ms), low coercivity (Hc) and remanence magnetization (Mr) values of these materials make them particularly suitable for data recording.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.