Abstract

We have grown CdS films by the Close Spaced Vapor Transport technique under specific conditions: substrate temperature ( T s ): 450 °C, source temperature ( T so ): 725 °C, argon pressure in the chamber ( P Ar ): 100, 200 and 500 mT, deposition time ( t d ): 100 s. The films were studied by measuring the luminescence properties at different temperatures in the range 10–300 K. The room-temperature PL spectrum of the as-grown CdS films showed a very broad band centered at 2.26 eV and a shoulder in the low-energy side at 1.80 eV. After CdCl 2 thermal annealing at 300 K, the spectrum showed better PL characteristics: a strong band in the low-energy side at 1.67 eV and a band in the high-energy side at 2.47 eV. The analysis at lower temperatures showed that the high-energy band becomes most intense and shifts to higher energies reaching a value of 2.54 eV, very close to the energy band gap at 10 K. The low-energy band becomes broader and centered around 1.9 eV. Analysis of the PL intensity as a function of temperature in an Arrhenius representation, allows applying a theoretical model for the quenching of the PL intensity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.