Abstract
Room temperature photoluminescence (PL) from plasma-polymerized hexamethyldisiloxane (PP-HMDSO) thin films deposited on silicon wafers has been investigated as a function of both the applied RF power and the monomer flow rate. Films were deposited in a low pressure–low temperature remote plasma ignited in a 13.56 MHz hollow cathode discharge reactor, using pure HMDSO as a monomer and Ar as a feed gas. The substrate temperature during the deposition was as low as 40 °C and the total pressure was about 0.03 mbar. Optical emission spectroscopy (OES) has been used as in situ tool for monitoring the different chemical species present in the plasma during deposition processes. The deposited PP-HMDSO films showed a strong, broad ‘green/yellow’ PL band. The RF power and the flow rate of the HMDSO monomer are found to have a significant impact on the PL intensity of the deposited film. The changes in the chemical bonding of the film as a function of deposition parameters have been investigated by using the Fourier transform infrared (FTIR) spectroscopic analysis and are related to PL and OES results. The ‘green/yellow’ PL band is ascribed to chemical groups and bonds of silicon, hydrogen and/or oxygen constituting the films, in particular, SiH, SiO bonds and silanol Si–O–H groups.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.