Abstract
Bisphenol A (BPA) is an endocrine disruptor, and removing it from contaminated water is a major environmental concern. Herein, graphene derivatives such as graphene (G), graphene oxide (GO), and reduced graphene oxide (rGO) supported silica-zirconia (SZ) were successfully synthesized for photodegradation of BPA. The photodegradation of BPA was ordered as follows: rGO/SZ (88%)>GO/SZ (63%)>G/SZ (58%)>SZ (55%). This is because rGO has bigger regions for π-π stacking and less negatively charged carboxyl groups, which BPA has a higher adsorption affinity than GO. In addition, the highest degradation is predominantly due to the high number of carbon-support interactions and defects sites, including oxygen vacancy. This encouraged effective mobility of charge carriers and subsequently enhanced photoactivity. In this study, the rGO/SZ catalyst was chosen to optimize further the reaction parameters including catalyst dosage, pH and initial concentration of BPA. According to the analysis of variance, the catalyst dosage was the most important variable in the degradation of BPA, followed by pH and initial concentration. The optimum BPA degradation predicted from response surface methodology is 88% at conditions of 8.09 mg L−1 using 0.469 g L−1 of rGO/SZ at pH 6.1, which is reasonably close to the predicted value (89.8%). The rGO/SZ catalyst was found to be stable even after five cycles in the reusability testing.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.