Abstract

Results of in-plane and out-of-plane thermal conductivity measurements on $\rm La_{1.8-x}Eu_{0.2}Sr_xCuO_4$ ($0\leq x\leq0.2$) single crystals are presented. The most characteristic features of the temperature dependence are a pronounced phonon peak at low temperatures and a steplike anomaly at $T_{LT}$, i.e., at the transition to the low temperature tetragonal phase (LTT-phase), which gradually decrease with increasing Sr-content. Comparison of these findings with the thermal conductivity of $\rm La_{2-x}Sr_xCuO_4$ and $\rm La_2NiO_4$ clearly reveals that in $\rm La_{2-x}Sr_xCuO_4$ the most effective mechanism for phonon scattering is impurity-scattering (dopants), as well as scattering by soft phonons that are associated with the lattice instability in the low temperature orthorhombic phase (LTO-phase). There is no evidence that stripe correlations play a major role in suppressing the phonon peak in the thermal conductivity of $\rm La_{2-x}Sr_xCuO_4$.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.