Abstract
The phase-specific high temperature creep behaviours of the γ and γ′ phases of a rafted Ni-based single crystal superalloy were investigated by a combination of in situ creep experiments and diffraction of high-energy X-ray synchrotron radiation. In situ experiments were performed at constant temperatures in a 930–1125 °C temperature range and under variable applied stress in order to study the material’s response (plastic strain, load transfer) to stress jumps. Using three crystal diffractometry in transmission (Laue) geometry, it was possible to measure the average lattice parameters of both the matrix and the rafts in the [1 0 0] direction at intervals shorter than 300 s. The absolute precision on the measurement of the constrained transverse mismatch (in the rafts’ plane) is better than 10−5. Plastic strain occurs within the γ corridors as soon as the Von Mises stress exceeds the Orowan stress. The plasticity of the γ′ rafts apparently depends on the transverse stress (i.e. perpendicular to the tensile axis) exceeding a threshold value of 60 MPa.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.